After-sales Service: | Warranty |
---|---|
Warranty: | 1 Year |
Certification: | ISO 9001:2000, ISO 9001:2008 |
Manufacturing Process: | Woven |
Material: | Polyester |
Condition: | New |
Customization: |
---|
Suppliers with verified business licenses
type | feature | Application scenarios |
Single layer/1.5 layer | Dehydration soon Large difference on both sides Poor wear resistance |
Kraft paper corrugated paper |
2.5 layer | Slow dehydration Good paper quality Wear resistance Long service life |
Various grades of paper |
Triple layer | Uniform dehydration High retention rate Good paper quality |
Various grades of paper |
2.5 layer Forming Fabric | ||||||||
Fabric Code | Warp Mesh | Weft Count | Warp Diameter | Weft Diameter | Air Permeability/m3/m2h CFM | FSI | DI | |
SH2B6408 |
71.5-72.5 | 67.5-68.5 | 0.15 | 0.18 0.12/0.22 0.22 | 4350 | 275 | 155 | 25.7 |
71.5-72.5 | 65.5-66.5 | 0.15 | 0.18 0.12/0.22 0.22 | 4600 | 290 | 152 | 26.3 | |
71.5-72.5 | 56.5-57.5 | 0.15 | 0.18 0.12/0.22 0.22 | 5800 | 370 | 135 | 29.0 | |
71.5-72.5 | 47.5-48.5 | 0.15 | 0.18 0.12/0.22 0.22 | 7900 | 500 | 119 | 33.0 | |
SH2B5616 |
62.5-63.5 | 60.5-61.5 | 0.17 | 0.20 0.13/0.30 0.30 | 4500 | 285 | 139 | 23.9 |
62.5-63.5 | 59.5-60.5 | 0.17 | 0.20 0.13/0.35 0.35 | 3950 | 250 | 137 | 20.6 | |
62.5-63.5 | 53.5-54.5 | 0.17 | 0.20 0.13/0.35 0.35 | 5050 | 320 | 126 | 23.7 | |
62.5-63.5 | 47.5-48.5 | 0.17 | 0.20 0.13/0.35 0.35 | 6000 | 380 | 115 | 25.1 | |
SH2B4216 |
47.0-48.0 | 47.0-48.0 | 0.22 | 0.22 0.13/0.35 0.35 | 6000 | 380 | 107 | 25.1 |
47.0-48.0 | 40.0-41.0 | 0.22 | 0.25 0.17/0.40 0.40 | 7000 | 445 | 94 | 25.1 | |
SH2B3616 | 40.5-41.5 | 38.5-39.5 | 0.26 | 0.30 0.20/0.50 0.50 | 5500 | 350 | 89 | 18.8 |
40.5-41.5 | 36.5-37.5 | 0.26 | 0.30 0.20/0.50 0.50 | 6350 | 400 | 85 | 20.4 | |
40.5-41.5 | 34.5-35.5 | 0.26 | 0.30 0.20/0.50 0.50 | 7000 | 445 | 82 | 21.4 |
Problem:
The mesh edge is worn too fast.
Solutions:
1. Try to increase the staggered width of vacuum box openings in turn.
2. Add normal pressure lubricating water to the edge of the vacuum box.
3. Apply stiffeners at appropriate positions.
4. Check whether the edge wiper plate and vacuum box have edges or gaps. In particular, the joint of the ceramic panel is a weak link.
5. Check whether the edge of each roll is seriously worn (the diameter becomes thinner after wear, so that the tension of the mesh is smaller than that of the normal mesh surface, further accelerating the wear)