The measured co-efficient of friction for material is 0.08 which comp- ares very favouralby with other plastics where the friction is between 0.16 and 0.20,or cross grain wood of 0.3.
Faster machine speeds can be achieved through the low coefficient of friction.˙ Less motive power required to drive machines.
The material has a high impact strength and cannot break or splinter . Temperature resistent to 1000C.
1.Excellent self-lubricating performance;
2.Good in resisting impact, flexibility;
3.Being excellent in resisting chemical corrosion(acid, alkali, salt);
4.Being free from toxin, smell or exudates;
5.Good electric resistance;
6.Low in water absorption;
7.Low coefficient of friction;
8.Resisting environment and anti-aging;
9.Resisting high and low temperature;
10.UV resistance
11.Extremely high anti-abrasion.
Property | Unit | Value |
Density | g/cm3 | 0.93-0.96 |
Average molecular weight | g/mol | 3million- 10 million |
Tensile strength (23°C in air) | MPa | 22 |
Breaking strength | MPa | 42 |
Tensile strain at break | % | 600 |
Ball indentation hardness | N/mm2 | 42 |
Shore D hardness | -- | 65-70 |
Abrasion | % | 70-80, steel = 100 |
Water Absorption | -- | NIL |
Temperature resistance | °C | -269 to +85 |
Melt Temperature | °C | 130-140 |
On paper and pulp industry